Molecular Formula | H2O |
Molar Mass | 18.01528 |
Use | Use for painting the exterior wall of high-rise buildings. |
The production of this coating adopts ball mill, fast grinding, high-speed dispersing machine or sand mill, etc. First, water, color filler, preservative, colorant and defoaming agent are added to the reactor for high-speed dispersion, then thickener and dispersant are added, stirred at high speed for 30min, then the rotating speed is reduced, antifreeze acrylic emulsion and wetting agent are added, stirred for 30min, filtration, discharging and packaging are carried out.